Steel surface treatment selectorTeräsrakenteiden pintakäsittelyvalitsin

Pick a zone and a fire requirement for each steel member. The page works out the corrosivity category, durability, preparation grade, corrosion system, fire protection and intumescent exposure type, warns about the combinations that go wrong, and writes the drawing side text in Finnish and English, line by line.

01

The algorithm

Corrosion protection and fire protection are specified by different people at different times, and that is where specifications go wrong. The fire system dictates what may sit underneath it, and the corrosion system dictates whether the fire protection can go on at all. Both tracks meet at step 6 before anything is written on a drawing. The tool below runs exactly these steps.

Member group on the GA drawing truss · column · hanger · stair · canopy · plinth · façade steel CORROSION TRACK FIRE TRACK 1Locate the member Heated interior · cold or humid interior · sheltered exterior · exposed exterior · salt splash at grade 2Corrosivity category EN ISO 12944-2 → C1 … C5 on a boundary, the more onerous category 3Maintenance access Limited access ⇒ at least H No access ⇒ VH: the first system is the only one 4Durability and preparation grade EN ISO 12944-1 → L ≤7 · M 7–15 · H 15–25 · VH >25 a P3 for painted C4–C5 with H/VH (ISO 12944-3 §5.5) 5Protection family Paint · HDG · duplex. HDG life check: zinc µm ÷ zinc loss rate ≥ durability, otherwise duplex AIs there an R requirement? The fire engineer confirms it per member group. Not every steel member has one. BCheck it unprotected first EN 1993-1-2. If adequate: no fire protection, and the corrosion track is free to galvanize CProtection type Thin-film intumescent · board · encasement · concrete filling of hollow sections DExposure type EAD 350402 → Z2 dry interior · Z1 humid interior · Y sub-zero or semi-exposed · X weather-exposed Eθa,cr and section factor → DFT The engineer issues critical temperatures; the supplier reads the DFT off the ETA for each A/V protection family fire system + exposure type 6 Reconcile the build-up: substrate → primer → intumescent → topcoat Intumescent means a paint system, not HDG, unless the ETA covers galvanized steel. Is the primer on the approved list? Does the topcoat suit UV and the category? not compatible → revise 5 … or revise C 7Detailing checks Vent and drain holes · slip factor class · dissimilar metals · galvanizing bath length · no epoxy topcoat in sunlight · fastener coatings · masking of contact faces 8Write it on the drawing Member tag, e.g. C2/VH R60 Z1 · side text in Finnish and English, the same lines in the same order
Two tracks, one build-up. The dashed returns matter most: when the intumescent approval does not cover a galvanized substrate, either the corrosion decision at step 5 changes or the fire protection type at C does.
02

Project inputs

Everything that goes on the drawing but is not decided per member. Type side-text values in capitals, the way they should appear on the drawing. The steel, fastener, welding and fire-protection notes are standard text, written into the side text for every project.

Your edits are kept in this browser only. Use Export to keep a copy with the project files or to pass it to a colleague.

03

Elements

One row per member type. Leave the category override empty unless the member really differs from its zone (a beam crossing from the foyer to the exterior takes the more onerous category). The unprotected check applies only when there is a fire requirement.

Output language
#ElementZoneCat. overrideFireUnprotected checkVisibleAccessLength mt mmSystem override
04

Results

The tag is what goes next to the member on the drawing. Coating thicknesses are indicative (EN ISO 12944-5 Annex C); the final system is the manufacturer's certified one, and the intumescent DFT comes from the supplier's ETA.

#ElementCat.Dur.PrepFire protectionExp.SystemIndicative build-upFastenersDrawing tagWarnings
05

Side text

Built from the project inputs and from what actually occurs among the elements: an unused category, system or fire rule leaves no line behind. Both versions have the same lines in the same order, and long notes are wrapped to 64 characters.

Copy format

Suomi

English

Pasting into AutoCAD. Aligned text goes straight into MTEXT; use a monospaced font if the columns should line up. Tab-separated text pastes into Excel as three columns and into an AutoCAD table via Paste Special as text. With ASCII only, restore the special characters on the drawing afterwards.
06

Reference tables

The values the tool uses. Corrosion rates and HDG thicknesses are from the standards; NDFT values are the indicative Annex C examples and must be confirmed against the chosen manufacturer's system.